+ Reply to Thread
Page 1 of 12 1234511 ... LastLast
Results 1 to 10 of 112
Tips and Tricks in Forum Suppliers; post your tips and tricks for all e-cigs here we can all learn from each others experiences....
  1. #1
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Smile Tips and Tricks

    post your tips and tricks for all e-cigs here

    we can all learn from each others experiences.
    ** fallen∞**

  2. Advertisement
  3. #2
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Default Refilling the Carty's

    This is the best method I have seen so far

    thanks to DogsBody for this

    it is Brilliant --------


    YouTube - Refill Ecig Cartos Quick and Easy (CCFM)
    ** fallen∞**

  4. #3
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Default Metal polishes


    Thanks to stormy for this one ----

    make us all shiny and lovely clean threads too ----


    Metal polishes
    I went to Ace today and they had a sale. I bought some Nevr-Dull, Maas and some Cape Cod metal polishing cloths. I already had some Noxon. Well after testing all four the Cape Cod polishing cloths worked better for me. It was easier and had a nice smell. They are pre-moistened clothes in a little zip pouch. I was surprised that they worked the best but they did. It was pretty cheap too. I will likely still use my jewelry cloths for a daily wipe though.
    ** fallen∞**

  5. #4
    Senior Member ECF Veteran DMertz99's Avatar
    Join Date
    Nov 2009
    Location
    Maryland
    Posts
    159

    Default

    I use Noalox joint compound on the threads of my Indulgence.

    IDEAL INDUSTRIES, INC. - Noalox® Anti-Oxidant Compound

    Helps eliminate cross-threading. Lowes has it in the .5 oz size. Look in the electrical isle.

    You can also find Permatex Anti-seize at most auto parts and hardware stores.

    Permatex 81343 Anti-Seize Lubricant 133 from the Oil & Fluids section of the Blazen Auto Store
    Never take life seriously. Nobody gets out alive anyway.

  6. #5
    Full Member
    Join Date
    Aug 2009
    Posts
    17

    Default

    If you find carty's aren't working on the indulgence, it's possibly a pre-ship coating that seems to be put on the threads. I've had four or five now that just don't spark up, but a few scrapes at the threading with something sharp and in comes the vapour.

  7. #6
    Senior Member ECF Veteran
    Join Date
    Jan 2010
    Location
    Australia
    Posts
    286

    Default

    For cleaning attys and cartos:

    YouTube - Carto-Miser

  8. #7
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Default

    hahahahah, DB,

    I was just going to post this in here for you - hahahahah

    you beat me to it -
    ** fallen∞**

  9. #8
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Default My Atty Resurrection Method

    This is the method I use for my attys also-----


    this from HighPing -------

    My Atty Resurrection Method



    This is the only method I use, and I have attys that are 4-5 months old and still going strong. One in particular, I have vaped well over 300ml through and it hits like the day (after) I got it

    1. Blow out any excess juice.
    2. Rinse with hot water and blow out thoroughly. (no need to dry over night, or anything. They have a built in dryer )
    3. Connect to battery...preferably something higher voltage than stock. I use my variable voltage power supply that's connected to a PS passthrough and set it to about 5.2V for a 510 (6.5ish for an 801), but if all you have is stock, then that will work too.
    4. Push button until you see orange hot...carefully...not super bright (white hot).
    5. Let off button and blow down the barrel (from a distance, not with your mouth actually on it), this kind of flash cools it and also gets some of the moist air out to speed the drying process.
    6. Repeat (steps 4 and 5) 5-10 times... you will see that gradually (once you've got it dry) the glow will occur much quicker.
    7. Once you have it to this point, press and release the button at a rate that just holds the orange glow (kind of a manual 'pulse width modulate'). Keep this glow going for 20-30 seconds, being very careful to maintain the glow at low orange (not bright red/white) or you'll pop it.
    8. Once you have done that, repeat steps 2-7 one more time.

    At this point you will have an atty that performs like (or better than) brand new. I have used this technique with 510, 801, 901, 401, and 4081 attys and it always works for me. I like this method because it is quick and simple. No need for any cleaners or overnight soaking. Takes 2-3 minutes and you're back in business.

    ** You do have to use some caution, as you can pop an atty pretty easily until you have the method down. I haven't popped one in quite some time though.

    **Also, no need to remove the wick (that's in there for a reason), as you are baking all the gunk out when you do this. This is the reason for the second rinse in the middle of the process. You basically turn the gunk to ash with the sustained orange glow, then rinse the ash out.

    If anyone tries this, give some feedback and let me know if you find any ways to perfect this method. Seems to work great, but there are always ways to improve

    Edit: (some tips on the "rinse, dry and burn" stages of the process)

    **Tips on the 'rinse' stage (step 2)
    Step 2 is meant to get as much juice out of the atty as possible. The more juice you can get out with the water rinse, the faster you will get the atty dry in steps 4&5. (The water will evaporate off much quicker than juice.)
    - Rinse by just running hot water from the tap first. Then once you have it somewhat clean, fill the atty barrel with water then (before all the water runs out), put it in your lips and blow the water through really hard. This will give all the nickel foam that's in the atty a kind of "power wash" and get most of any remaining juice out.

    **Tips on the 'dry' stage (steps 4 & 5):
    Steps 4 and 5 are meant to get the atty 'bone dry', before you move on to step 6 and the button pulsing.
    -The more water you can blow out before connecting to the batt, the better. Blow through the atty really hard from both ends (not at the same time)
    - You can also blow gently down the barrel (from a distance), while holding the button in step 4 to speed the drying process. This will clear the hot moist air out of the atty and allow for a quicker drying time. The key in these steps is to get the atty dried out.

    Tips on the 'Burn' stage (step 7)
    The whole key to not popping the atty is keeping a good visual on the coil, and watching the hottest part while pulsing the button. I have had a few attys that will get bright hot on one end of the coil and nothing on the other end of the coil. The way to make this method the most effective is to maintain that orange glow at the hottest end while pulsing the button. If you keep it up long enough you will see the glow slowly migrate across the coil. When you are all done the entire coil should glow when the button is pressed.
    Once you are past the drying step, you should not hold the button for more than one second. It should really be much shorter than that. More like a button pulse of 2-3 times a second.
    ** fallen∞**

  10. #9
    Di
    Di is offline
    ECF Veteran ECF Veteran Di's Avatar
    Join Date
    Oct 2008
    Location
    *Australia*
    Posts
    8,872

    Default Cartridge wool filler

    I have a little tip here I discovered quite by accident-----

    when you use a new cartridge it is great and vapes good,

    but I noticed some of them are packed really tight.

    I take out the filler and wash it with hot water, pat it dry on a paper towel,
    then pull it out and fluff it up,---

    then--

    remove about half of it --

    fluff it, cut the top end nice and straight

    and put it back into the cartridge, when you use it now,
    you will see it holds more juice,
    and vapes like a steam train.
    ** fallen∞**

  11. #10
    Super Member ECF Veteran bluesuede's Avatar
    Join Date
    Sep 2009
    Location
    Central PA, USA
    Posts
    833

    Default

    Great thread! We should sticky this!
    EM801, M401, KR8/DPV9/VK, Indulgence 3.7v & 6v, 510/LR510/510 cartomizers, RiVa, Leo.
    Smoke-free since 9/21/2009!

+ Reply to Thread
Page 1 of 12 1234511 ... LastLast

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

SEO by vBSEO