I prefer the durability of stainless cause if I drop it I would rather my carto, atty, etc. to break off and not my PV's threads it's cheaper that way. Now if your delivery device is also stainless steel than it's a crap shoot but still better than aluminum PV with a stainless tank that would surely ruin the threads on the PV.
 

alicuben

New Member
Mar 19, 2013
4
1
38
USA
Too post today to read ...
17.jpg





01.jpg
28.jpg
03.jpg
05.jpg
 

NancyR

Account closed on request
ECF Veteran
Apr 25, 2012
7,927
13,419
Washington State
The case material should have nothing at all to do with the voltage.

actually the case material plays an important part with the voltage, as with a mechanical mod the body is your ground so if it can't flow properly the mod will not work as it should if it works at all
 

tj99959

ECF Guru
ECF Veteran
  • Aug 13, 2011
    15,116
    39,600
    utah
    Actually it's the metals that actually touch the battery that can make a huge difference (contacts), but ask the ZEN folks about the copper screws if you think the metals used doesn't make a difference elsewhere. Any VV type PV worth it's salt should self adjust for any internal resistance, but mechanical mods can't. Ask those that bought an Apollo a year or so ago about the SS switches. The metal used to make the actual tube shouldn't make a big enough difference to ever notice, but the same metals used elsewhere in the PV could make the difference of working or not working at all.

    Having had both SS and chrome PV's, I like the SS. The chrome is a finger print magnet, and feels slippery.
     
    Last edited:

    DaveP

    PV Master & Musician
    ECF Veteran
    May 22, 2010
    16,733
    42,646
    Central GA
    Chrome is a coating that can chip and flake if dinged. Aluminum is generally too soft to resist dings. Stainless steel is solid through and through and will look far better in a year or two than either of the above. The down side is that is heavier, but it doesn't take long for SS to feel normal. Anything else feels like a toy after handling a SS mod.

    If SS is good enough to withstand the pressures in a firearm, it's good enough for my ecig mod tube.
     

    tj99959

    ECF Guru
    ECF Veteran
  • Aug 13, 2011
    15,116
    39,600
    utah
    Chrome is a coating that can chip and flake if dinged. Aluminum is generally too soft to resist dings. Stainless steel is solid through and through and will look far better in a year or two than either of the above. The down side is that is heavier, but it doesn't take long for SS to feel normal. Anything else feels like a toy after handling a SS mod.

    If SS is good enough to withstand the pressures in a firearm, it's good enough for my ecig mod tube.


    I don't know of any SS PV's with a 5-10mm wall thickness, so I doubt that you would find any that could withstand the pressures of a firearm.
     