The seams between all of the tubes are virtually imperceptible. I got the matte/brushed finish.
That's WHY the seams are virtually imperceptible.
In contrast, my two polished Nemesis' have a very visible seam between the tubes.
The polishing process causes that. Pretty much every polished mod I've see has that characteristic. The buffer surface pressure is released at the edge, overhangs the edge, and works it harder, causing more wear around the edges. Only way I can think of avoiding that would be to polish all tubes assembled (but you'd still have a top and bottom edge, so you'd see a seam at the atty/top cap connection).
Trying to find 17mm tank atomizers for this now, but am having a hard time.
I'm using the IGO-S with 17mm Cap-It-All. Looks decent for now, until Atmomixani release a Nemi atty. The brushing on the cap isn't quite the same as the Nemi, but blends better than a polished atty would.
PS - http://ukvapers.org/Thread-coming-soon-from-Atmomixani?pid=759240#pid759240
Last edited: